VihoX-760 three-station line, PP takeaway containers, cleanroom production room.
Thirty-seven seconds is long enough to see whether a line is under control. The sheet crosses the heater bank, is formed and trimmed inside one welded frame, and lands on the discharge belt as a nested stack of white PP takeaway containers. Two operators count and carton it.
That is the argument for three stations: a single-station former can make the same box, but not to the same wall tolerance and lip, at that rhythm with two people at the line end.
What the 37 seconds show, and what they do not
- 0:00–0:05, unwind. Film enters under tension; the dancer arm takes up slack each time the chain indexes.
- 0:05–0:12, heat. Ceramic zones sit above and below the sheet plane; only the rails touch the web, so edge heat loss is its own problem.
- 0:12–0:22, form and trim. The upper platen descends, positive air is admitted, the lower cavity pulls vacuum. Trimming happens at a separate station downstream.
- 0:22–0:37, discharge. Trimmed containers land on the belt, are nested by hand and packed into cartons.
The clip cannot tell you the HMI cycle time or the cavity-by-cavity weight spread from a first-article report. Ask for both before approving a tool drawing.
Why 760 mm is the practical width for takeaway work
Width drives cavity count, die size, tonnage, heater load and skeleton weight. At 760 mm you can run four 1000 ml boxes or twelve 750 ml boxes across the web once the rails and trim border are deducted: enough to justify three stations, without the die cost and web sag of a 900 mm line. Drop to 600 mm and a third of the cavities disappear for the same labour and connected load.
| Parameter | Value | Why it matters at the packing table |
|---|---|---|
| Usable sheet width | 760 mm | Sets cavity count across the web and trim die width |
| Forming area | up to 760 × 520 mm | 4-up 1000 ml boxes, 12-up 750 ml boxes, 9-up bento trays |
| Stations | 3: forming, trimming, discharge | Die wear never disturbs the forming pressure recipe |
| Sheet gauge | 0.30 – 1.50 mm | Most takeaway walls sit between 0.5 and 0.9 mm |
| Maximum draw depth | up to 160 mm | 65–75 mm boxes through 110 mm soup bowls |
| Clamp / trim force | 35–50 t / 40–60 t | Holds the pressure seal and shears a multi-cavity perimeter |
| Forming pressure / vacuum | 0.4–0.8 MPa / −0.06 to −0.09 MPa | Six to eight times the driving force of vacuum alone |
| Heating zones | 4–6 upper + 4–6 lower, SSR | Rail-clamped edges run hotter than the centre to compensate for chain loss |
| Cycle band (reference) | 10–28 cycles/min | A band, not an output figure; depth, gauge and cooling decide |
| Connected load / water | 65–90 kW / 12–18 °C at 12–20 m³/h | Heaters dominate the bill; mold temperature sets warpage and cycle |
Station one: heat, and the sag you have to plan for
PP at 0.7 mm sags 8–12 mm across a 700 mm span once the surface passes roughly 140 °C. That is not a fault; it says the profile is ahead of the chain index. Drop the setpoint and you form a cold box with stress whitening at the corners.
The rails clamp about 30 mm of sheet each side, that strip loses heat into steel every index, so the edge zones run 8–12 °C hotter than the centre. Two checks: an offcut from the rail edge should droop at the same rate as one from the centre at the oven exit, and the SSR duty cycle should settle after twenty minutes instead of sawtoothing.
Station two: what negative-positive pressure buys
Vacuum alone gives about 0.09 MPa of driving pressure; air at 0.6 MPa gives roughly seven times that, the difference between a 6 mm corner radius and a 3 mm one on the same tool. A shallow 500 ml box with generous radii is fine on vacuum. A compartment tray with 5 mm internal corners is not: the sheet bridges, the base radius thins, and the part only fails when a customer stacks it four high.
Sequence matters more than the headline number. Pre-stretch with the plug, seal the cavity, draw vacuum to release the sheet, then admit air. Pressure before evacuation traps air and leaves a glossy blister on the base — a defect that appears at the packing table, not at the machine. Plug clearance runs 0.3–0.6 mm at the deepest point: too tight drags material, too loose pre-stretches nothing.
Station three: trim separately, and judge it at the lip
On a single-station machine the trim die shares the forming platen, so forming tonnage competes with the trim and every die nick changes the pressure. Splitting the stations sends the sheet to a dedicated press with its own guide columns: sharpening the die never touches the forming recipe.
Food containers are judged at the lip. A burr above 0.1 mm stops a lid seating and cuts a glove within the hour. We grind matched-metal dies to 0.02–0.04 mm clearance per side, harden to HRC 58–62, and check the lip on a profile projector at first article and after every die service. If a part hangs, check lip cooling and blocked vacuum holes before the ejector.
Container geometry decides whether the line runs or fights you
Most problems we fix were designed into the container, not the machine. This is the checklist we run before a tool drawing is released.
| Feature | Workable range | What happens outside it |
|---|---|---|
| Draw ratio (depth : width) | up to 0.8 : 1 with plug assist | Base thins below 40% of nominal and corners web |
| Base corner radius | 4–8 mm | Under 3 mm the sheet bridges and the corner turns translucent |
| Draft on side walls | 3°–7° | Under 2° the part drags on ejection and the rim distorts |
| Lip width | 5–9 mm flat land | Narrow lips curl under heat-seal pressure; wide lips waste sheet |
| Web bridge between cavities | 8–12 mm | Below 6 mm the skeleton tears during indexing and the chain stalls |
Changeover: 750 ml to 1000 ml inside one shift
With two fitters and a crane: cool and purge 20 min; disconnect water and air on quick-couplers 10 min; roll the tool out and the new one in 40–60 min; reset rail width and index pitch 20 min; align the trim die on its pilot pins 30–45 min; recall the recipe and soak 30 min; first article on weight, lip, depth and stack height 20 min.
Three to four hours the first time, two and a half once practised. Anyone quoting thirty minutes is describing a different machine or an exchange die set most takeaway projects will not pay for. Ask for the video.
Material behaviour on the same tool
A 760 frame runs PP, APET, PS and PLA, but not on one recipe and not to one lip dimension. The heat window decides whether a container is a food box or scrap.
| Resin | Sheet surface | Mold temp | Best fit and limit |
|---|---|---|---|
| PP | 135–165 °C | 20–30 °C | Hot fill, microwave, delivery; shrinkage 1.2–2.0% |
| APET | 115–140 °C | 10–20 °C | Cold display, clarity; narrow window, brittle lip if overcooled |
| PS | 125–150 °C | 20–30 °C | Chilled short-shelf food; no hot fill, no microwave |
| PLA blends | 110–135 °C | 15–25 °C | Compostable positioning; deflects above 55 °C |
Energy, and what a thousand boxes costs to run
Buyers are rarely surprised by the machine price, but the heaters draw power whether or not the chain indexes. A 760 platform meters at 40–60% of connected load in steady production on 0.7 mm PP, so budget 30–50 kW; slowing the cycle barely moves it, which makes energy per part worse.
The arithmetic: a 15 g box on a twelve-cavity tool at ten cycles per minute gives 7,200 impressions an hour, 85–92% saleable. Electricity lands at 5–8 kWh per 1,000 boxes and compressed air at 6–10 Nm³, before two operators and a packer.
FAT: what to witness before the balance leaves
- Run time. Eight continuous hours on your resin; twenty-four if the tool serves a chain account.
- Cavity weights. Weigh every cavity twice at steady state and ask for the sheet: max-to-min inside ±3%. An average hides the starved cavity that fails your customer’s fill check.
- Cycle and lip. Thirty-minute log drifting under ±0.5 s; burr under 0.1 mm; lip flatness within 0.15 mm; 50-piece stack within ±1.5 mm.
- Metered utilities. Clamp, flow and air meters; those readings are your cost model.
- Documents. Electrical and pneumatic drawings, spare list with lead times, HMI recipe backup, cavity-numbered tool drawing, signed report with both serial numbers.
Insist on your own sheet lot: two rolls of the same grade from different extruders can shift the forming window by 5–8 °C.
Before the frame lands
The frame stands about 2.6 m and will not pass a standard 2.1 m cleanroom door, so plan panel removal and crane reach before the truck loads. Then confirm a slab rated for roughly 10 t and level within 3 mm over 3 m, three-phase supply sized to connected load, chilled water at 12–18 °C with 100 µm filtration, an air receiver of at least 1 m³, and 760 mm sheet on 76 or 152 mm cores. Fix the unwind side at order; reversing it later is a rebuild.
Where this line fits
The 760 suits a converter running 2,000–8,000 containers an hour across two or three SKUs in PP, APET or PS. A single-SKU plant that will never change a tool is better served by a vacuum former plus a separate cutting press. For the structural difference read what a three-station machine is, for commercial questions the three-station buyer FAQ, for formats the takeaway container page, and for full scope the food container production line.
Frequently asked questions
1. Do I need a three-station line, or is a single-station vacuum former enough?
Depends on corner detail. Shallow boxes with generous radii run on vacuum. Once the design has compartment corners under 6 mm, a reinforced rim or a measured trim tolerance, the trim press is cheaper than the rejects.
2. How long does a mold change take, and what shortens it?
Three to four hours first time with two fitters, two and a half once practised. Pre-set manifolds, a mold cart and stored recipes cut the most; a second trim die set saves most on weekly switches.
3. Can one tool run both PP and APET?
Mechanically yes. APET forms 20–25 °C cooler and shrinks far less, so the same cavity gives a different finished dimension and lip feel. Where a lid must snap, cut separate tools or cut for the tighter resin.
4. Corner webbing and thin bases: what do I check first?
Check sequence before temperature. Webbing is usually pressure arriving before the cavity is evacuated, or a plug retracting late. A thin base with clean corners is a plug too cold or too deep.
5. What utilities must be ready before the machine arrives?
Roughly 65–90 kW connected load, 12–20 m³/h of chilled water at 12–18 °C, and 1.8–3.0 m³/min of dry air at 0.6–0.8 MPa with a receiver at the machine. Confirm against the schedule issued with your order.
6. What should I witness at FAT before releasing the balance?
An eight-hour run on your sheet lot, a per-cavity weight sheet inside 3%, a thirty-minute cycle log, lip burr under 0.1 mm, stack height within 1.5 mm over fifty pieces, metered utilities, and documents with both serials.
7. How many boxes per hour can I put in a business plan?
Cavities times a measured cycle, then 85–92%. Twelve cavities at ten cycles a minute is 7,200 gross, so plan on 6,100–6,600 saleable. Build on your slowest shift, not a demo cycle.
8. What must be in place downstream so packing is not the bottleneck?
A granulator close enough that the skeleton is not carried, a discharge belt at about 900 mm, and a carton spec agreed before the layout. Two operators keep pace only when cartons are within reach and count is fixed by a counter.
Talk to the people who cut the tool
Send the container drawing, resin, target output and a photo of the room. You will get a cavity layout, a cycle estimate with its assumptions, and a utility schedule.
- Manufacturer: VihoX Machinery — Shenzhen Weixin Plastic Machinery Factory
- Engineering WhatsApp: +86 147 7547 6896
- Official site: cupmachine1.com
- Factory: Shenzhen, Guangdong, China